    Priming with Powder - The legendary durability of powder-coated finishes is further enhanced with this epoxy based powder primer. If the utmost corrosion resistance and adhesion are important to you, you'll want to use this primer under every opaque powder we sell. (Not for use under our translucent finishes.) For best results apply to clean bare metal and place in a preheated 400-degreeF oven until flow out occurs. DO NOT cure beyond flow out as adhesion will be adversely affected. Remove from oven, cool, apply powder of choice and bake as normal.

    About Hotcoat Powder Gray Primer

    Priming with Powder - The legendary durability of powder-coated finishes is further enhanced with this epoxy based powder primer. If the utmost corrosion resistance and adhesion are important to you, you'll want to use this primer under every opaque powder we sell. (Not for use under our new line of High Temp Powders, or directly under translucent finishes.) For best results apply to clean bare metal and place in a preheated 400 degree F oven until flow out occurs. DO NOT cure beyond flow out as adhesion will be adversely affected. Remove from oven, cool, apply powder of choice and bake as normal.


    Contents

    One 8 ounce bottle, enough to cover about 10 sq.ft.


    Accessories

    Use PRE Painting Prep (10041Z) to remove residual grease or oil before powder application.


    FAQ

    Allowing the Epoxy powder primer to fully cure will cause poor adhesion of the top coat. Some degree of adhesion can be restored to fully cured epoxy primer by sanding with 220 grit paper, however adhesion is always best when the top coat is applied over the partially cured primer surface.


    Customers also viewed:

    Customer Reviews

    2 Item(s)

    per page
    Good product, poor instructions (Posted on 2/3/14)
    Review by Robert
    Price
    Value
    Quality
    I can't speak to the long term durability of this stuff yet, but it goes on nice and flows out well. However, the bottle has the wrong instructions on it. Online it says to let it flow out and remove from oven, let cool, and apply top coat. It says DO NOT cure longer than flow-out before putting top coat on. The bottle itself has the same label as all their powder, and says to bake for 20 minutes after flow-out.
    Definately increases adhesion, OK filler (Posted on 1/7/10)
    Review by mbramel
    Value
    Quality
    Price
    Based on my chip test (body hammer whacks) this does increase the adhesion pretty well. It sustained pretty much every solvent except for brake cleaner. It also works as a light filler, not like All Metal but enough to cover up the blast profile. Seems to work best when its just flowing out, then topcoat and fully cure